Sign In | Join Free | My himfr.com
Home > Invar 36 Material >

High Dimensional Stability UNSK93600 4J36 FeNi36 Invar 36 Rod

    Buy cheap High Dimensional Stability UNSK93600 4J36 FeNi36 Invar 36 Rod from wholesalers
     
    Buy cheap High Dimensional Stability UNSK93600 4J36 FeNi36 Invar 36 Rod from wholesalers
    • Buy cheap High Dimensional Stability UNSK93600 4J36 FeNi36 Invar 36 Rod from wholesalers
    • Buy cheap High Dimensional Stability UNSK93600 4J36 FeNi36 Invar 36 Rod from wholesalers
    • Buy cheap High Dimensional Stability UNSK93600 4J36 FeNi36 Invar 36 Rod from wholesalers

    High Dimensional Stability UNSK93600 4J36 FeNi36 Invar 36 Rod

    Ask Lasest Price
    Brand Name : BLM
    Model Number : BLM-1
    Price : USD18-20/KG
    Payment Terms : L/C, T/T
    Supply Ability : 100MT/moth
    Delivery Time : 10-30 work days
    • Product Details
    • Company Profile

    High Dimensional Stability UNSK93600 4J36 FeNi36 Invar 36 Rod

    Hot Sale Manufactures Expansion Alloy Stability Invar 36/4j36//Fe-Ni36/Unsk93600


    Invar 36 is used where high dimensional stability is required,such as precision insturmrent,such as precision instruments,clocks,seismic

    creep gauges,television shadow-mask frames,valves in motors,and antimagnetic watches.In land surveying,when first-order (high-precision)

    elevation leveling is to be performed,the level staff (leveling rod) used is made of Invar,instead of wood,fiberglass,or other metals.Invar struts were used in some pistons to limit their thermal expansion inside their cylinders.


    NiCrFeCMnSiCoPS
    MIN35
    MAX370.2Margin0.030.350.20.50.020.01

    Cold rolled stripHot rolled flat barHot forging barCold pulling wireCold pulling bar
    0.01-2.5 x1-4002.5-20 x 5-400Φ12-400x1000Φ0.05-2.0 x LΦ2.0-12 x L

    Tensile StrengthElongation
    Mpa%
    64114
    6899
    7318

    The heat treatment process

    Annealing for stress relief

    Heated to 530~550℃ and hold 1~2 hours.Cold down


    Annealing

    In order to eliminate hardening,which can be bring out in cold-rolled,cold drawing process.Annealing needs heated to 830~880℃

    in vacuum,hold 30min.


    The stabilization process

    1.In protrective media and heated to 830℃,hold 20mins.~1h,quench

    2.Due to the stress generated by quenching,heated to 315℃,hold 1~4h


    Precautions

    1.Can not be hardened by heat treatment

    2.Surface treatment can be sandblasting,polishing or pickling

    3.Alloy can be used 25% hydrochloric acid picking solution at 10℃ to clear oxidized surface.




    Quality High Dimensional Stability UNSK93600 4J36 FeNi36 Invar 36 Rod for sale
    Inquiry Cart 0
    Send your message to this supplier
     
    *From:
    *To: BLOOM(suzhou) Materials Co.,Ltd
    *Subject:
    *Message:
    Characters Remaining: (0/3000)